Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | |
3M 1080 Vinyl Film Dual cast vinyl film in an array of colors; Five distinctive-looking finishes-matte, satin, gloss, carbon fiber and brushed metal; Use the film right out-of-the-box without graphic protection; Press.. |
|||
Maximum Service Temperature, Air | 32.0 - 40.0 °C | 89.6 - 104 °F | Deflection Temp at unknown load |
Abatron AboCast 8502-6/AboCure 8502-6 Colorless, Low-Exotherm Epoxy Casting Compound AboCast 8502-6/AboCure 8502-6 is a flexible, colorless, low-exotherm epoxy casting compound for spherical masses up to 2000 grams. It is a 2-component structural and dielectric liquid system with lo.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves |
3M Controltac™ 180Cv2-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | |
3M Controltac™ 3690C Graphic Film with Comply™ Adhesive This is a 2-mil white, clear or black film for screen printing graphics. The aggressive, pressure activated-adhesive is slideable and repositionable, and has air release channels for fast and easy b.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves |
3M Controltac™ 8620 ES Conformable Graphic Film These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves |
3M Controltac™ 8620Cv2 ES Changeable Graphic Film with Comply™ v2 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves and/or watercraft |
3M Controltac™ FN180C-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | |
3M Scotchcal™ 3662 Graphic Film This is a 2-mil, durable, opaque film designed for making short term graphics that are applied to unsealed, outdoor, pedestrian traffic surfaces or selected smooth-to-rough wall surfaces. This film .. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | |
3M Scotchcal™ 3690 Graphic Film This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some lo.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | |
3M Scotchcal™ 3690LF Graphic Film This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some lo.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves |
3M Controltac™ 180C Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves |
3M Controltac™ 8620Cv3 ES Changeable Graphic Film with Comply™ v3 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves and/or watercraft |
3M Controltac™ FN180Cv3-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves and/or watercraft |
3M Controltac™ IJ180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves and/or watercraft |
3M Controltac™ IJ180C-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves and/or watercraft |
3M Controltac™ IJ180Cv3-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves and/or watercraft |
3M Controltac™ RG180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves and/or watercraft |
3M Controltac™ RG180C-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound Curves and/or watercraft |
3M Envision™ 480Cv3 Print Wrap Film High performance, 2-mil white, non-PVC film with a luster finish; Pressure-act adhesive for easy sliding, tacking, snap up and repositioning; non-visible air release channels for fast and easy, bubb.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | |
3M Scotchcal™ 8662 Graphic Film This is a 2-mil, durable, opaque film designed for making short term graphics that are applied to unsealed, outdoor, pedestrian traffic surfaces or selected smooth-to-rough wall surfaces. This film .. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves |
3M Controltac™ 180 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Maximum Service Temperature, Air | 32.0 °C | 89.6 °F | Compound curves |
3M Controltac™ 8620C ES Changeable Graphic Film with Comply™ Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |