Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 316 °C | 601 °F | |
Saint-Gobain Fluoroloy® A15 High Performance Seal Material Improved sealing at low pressure; Can be abrasive running against soft metals
Information provided by Saint-Gobain Performance Plastics. |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | |
3M 363L Specialty Foil Tape Linered version of 363Information provided by 3M |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | |
3M 363LC High Temperature Aluminum Foil/Glass Cloth Tape 3M™ High Temperature Aluminum Foil/Glass Cloth Tape 363LC can be used as a high temperature, heat reflective, protective wrap for certain cables and other components in aerospace and industrial app.. |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | |
3M 433 Premium Performance Aluminum Foil Tape Silicone adhesive for high temperature resistance; MIL-T-47014, FAR 25.853, UL 746C Recognized; smooth easy unwind; clean, straight edges with minimal wrinkling.Information provided by 3M |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | |
3M 433L Premium Performance Aluminum Foil Tape Linered version of 433Information provided by 3M |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | Operating Temperature |
California Fine Wire Stablohm 800 Nickel, Chromium, Aluminum, and Copper Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | Operating Temperature |
California Fine Wire Stablohm 825 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | Ductility loss due to carbon phase precipitation above this temp. |
ATI Allegheny Ludlum AL 200™ Nickel Alloy, UNS N02200 Ferromagnetic. Allegheny Ludlum AL 200 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c.. |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | |
3M 363 Specialty Foil Tape Aluminum foil/glass cloth. Highest temperature metal foil tape.Information provided by 3M |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | |
Saint-Gobain Fluoroloy® A30 High Performance PTFE/Glass Seal Material Excellent heat, wear, and chemical resistance; Good cryogenic properties; Can be abrasive running against soft metals at high surface speed; Excellent material for back-up rings
Information .. |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | Maximum recommended service temperature. |
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen.. |