Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 249 °C | 480 °F | Long Term |
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | Long Term |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | Long Term |
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | Long Term |
Quadrant EPP Ketron® CM 1030HT PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | Long Term |
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | Long Term |
Quadrant EPP Ketron® CM HPV PEEK Polyetheretherketone; PTFE, Graphite, and Carbon Fiber Filled Bearing Grade, compression molded (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | Long Term |
Quadrant EPP Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | Long Term |
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | Continuous |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | |
Quantum PEEK 30% Carbon Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | |
Technetics Group Amicon™ PEEK
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | |
Technetics Group Amicon™ PEEK 30% Glass Filled
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | |
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | |
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | |
Styrolution Zylar 960 MBS ZYLAR 960 is an impact modified styrene acrylic copolymer that provides toughness equivalent to some grades of polycarbonate, good clarity and superior processing characteristics for demanding injec.. |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | |
Styrolution Clearblend 145 MBS Clearblend 145 is an impact modified styrene acrylic copolymer blend with excellent clarity.Excellent clarityLow densityEase of processingLow moisture absorptionInformation provided by Styrolution |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | |
Styrolution Clearblend 165 MBS CLEARBLEND 165 is an impact modified styrene acrylic copolymer blend with excellent clarity and outstanding toughness.Exceptional toughnessLow densityEase of processingLow moisture absorptionInforma.. |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | |
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining.. |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | Long Term |
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho.. |
|||
Maximum Service Temperature, Air | 249 °C | 480 °F | |
Quantum PEEK Information provided by Quantum Advanced Engineering Plastics |