Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 236 °C | 457 °F | Heat Resistance; ASTM D570D |
Plenco 08225 Polyester BMC, Compression Molded PLENCO 08225 is a renumber of PlasGlas 20215. PLENCO 08225 is a 15% glass-filled polyester bulk molding compound characterized as a medium strength electrical grade, but has many outstanding propert.. |
|||
Maximum Service Temperature, Air | 236 °C | 457 °F | Heat Resistance; ASTM D570D |
Plenco 6015 Phenolic, Briquette, Transfer Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Maximum Service Temperature, Air | 236 °C | 457 °F | Heat Resistance; ASTM D570D |
Plenco 6990 Phenolic, Briquette, Injection Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |