Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 209 °C | 408 °F | |
3M Scotch-Weld™ RT40 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
Maximum Service Temperature, Air | 209 °C | 408 °F | Heat Resistance; ASTM D570D |
Plenco 1581 Polyester, Briquette, Transfer Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |