Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 171 °C | 340 °F | Long Term |
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet) Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it.. |
|||
Maximum Service Temperature, Air | 171 °C | 340 °F | |
Quantum PEI - Ultem® Information provided by Quantum Advanced Engineering Plastics |
|||
Maximum Service Temperature, Air | 171 °C | 340 °F | Long Term |
Quadrant EPP Duratron® PEI U1000 Extruded Unfilled Polyetherimide (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 171 °C | 340 °F | Long Term |
Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 171 °C | 340 °F | Long Term |
Quadrant EPP Semitron® 420 ESd V (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 171 °C | 340 °F | Short Term |
Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products
(discontinued **) ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and .. |
|||
Maximum Service Temperature, Air | 171 °C | 340 °F | Heat Resistance; ASTM D570D |
Plenco 1501 Polyester, Briquette, Transfer Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Maximum Service Temperature, Air | 171 °C | 340 °F | continuous |
Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative A static dissipative polyetherimide utilizing proprietary filler technology which renders this material electrically conductive. This technology allows for good dimensional stability after machinin.. |
|||
Maximum Service Temperature, Air | 171 °C | 340 °F | Short Term |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |
|||
Maximum Service Temperature, Air | 171 °C | 340 °F | Long Term |
Quadrant EPP Semitron® ESd 420- CM Dissipative Polyetherimide(ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 171 °C | 340 °F | |
Quantum PEI - Ultem® 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |