Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 155 °C | 311 °F | NEMA temperature |
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | NEMA temperature |
Glastic Laminates/Shapes UTS Fiberglass-Reinforced Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-2. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | Continuous |
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | IEC 60216-1, Tensile strength, 20000 h |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | Approximate temperature class |
Haysite EHC Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) This IEEE Class F 155ºC high strength material exhibits substantial resistance to cold flow or creep under heat and pressure. Suggested applications include motor slot wedges, washers, brush plat.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | Approximate temperature class |
Haysite H755 Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A new generation of IEEE Class F, 155ºC /165ºC NEMA GPO- 1 material. H755 is designed to bridge the gap between 130ºC Class B GPO-1 materials and Class H 180ºC grades. H755 has quickly g.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | UL temperature Index |
Sumitomo Bakelite Durez® 153 Phenolic, Compression Grade Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Von Roll Isola IMI Varnish 9522 Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 24°C. Average solids: 50%. Usage Notes: Treating transformers, magnet coils, stators, fields, armatures, railway field coils, bare copper coils, etc.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Zotefoams ZOTEK® F 40 HT LS PVDF Foam Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Zotefoams ZOTEK® F 40 HT PVDF Foam Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Eccobond® 11 Heat Cure Catalyst Emerson & Cuming 11 Eccobond® Heat Cure CatalystGeneral purpose, low viscosity, elevated temperature curing. Long working life. Yields cured coatings with excellent chemical resistance. Subject to .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Goodfellow Polyethylene Naphthalate (PEN) Film A polyester that is chemically quite similar to PET but which is more temperature resistant. So far available only as biaxially oriented and heat stabilized films, they are semi-crystalline and colo.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Eccobond® 1962-31 Needle Bonding Epoxy Adhesive Emerson & Cuming 1962-31 Eccobond® Needle Bonding Epoxy AdhesiveOne component, medium viscosity, epoxy needle bonding adhesive. Designed to bond stainless steel cannulae into polypropylene hubs. Al.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Stycast® 1090/11 Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Stycast® 2057FR/11 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Stycast® 2850FT-FR/11 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | IEC 216 |
Dr. D. Mueller Flexiso® DMD FI 14010 00210 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00210 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | IEC 216 |
Dr. D. Mueller Flexiso® DMD FI 14010 00240 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00240 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Cytec (Conap) FR-1047 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Cytec (Conap) FR-1210 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Cytec (Conap) FR-1610 / EA-039 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | IEC 216 |
Dr. D. Mueller Flexiso® DMD FI 14010 00360 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00360 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
ATG s.r.l. EPDM Ethylene-Propylene Terpolymer |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Stycast® 2651MM/11 Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Stycast® XT-1169 Two-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Von Roll Isola IMI Varnish 74030 Solventless Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >99°C. Usa.. |