Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1600 °C | 2910 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 55 S Dense Refractory Brick Description: This andalusite based brick is characterized by a low porosity and a good creep resistance (After 24 hours at 1350°C under a load of 0.2 MPa gives between 14th and 24th hour a creep .. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 HC Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast LP 60 AAP Dense Refractory Brick Description: Special low porosity quality for use under severe corrosive conditions, (for instance liquid slags). Moreover, this brick has been extra protected against slag attack because it also co.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast LP 85 M Dense Refractory Brick Description: A bauxite brick with a mullite bond with a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, outlet cement kilns, electric arc furnace roofs... |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast AK 85 M Dense Refractory Brick Description: A bauxite based brick with a mullite bond. Application: torpedo ladles, electric arc furnace roofs, cement kilns.Remarks: This data represents average values, obtained from samples that.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast VIBRON 160 K Dense Vibrating Refractory Castable Description: Vibron 160 K is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity and high abrasion resistance. The thermal shock resistance is excell.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics PCF80 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics REFCAST K High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics REFCAST LC70 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics VELECRETE RC 104 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | Continuous Use |
Goodfellow Alumina/Silica SiO2 20/Al2O3 80 A continuous multi-filament yarn similar to those made wholly from alumina, relative to which it has a lower upper-use temperature but is more flexible. Similarly, it is used for composites and ther.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Zircar Ceramics ECO-20AA Alumina Insulation ECO-20AA is most commonly utilized as hotface insulation in furnaces with hydrogen rich atmospheres such as bright annealing furnaces.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Zircar Zirconia Buster Blanket Alumina Blanket Insulation Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | No Load |
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Chosun Refractories 1600BLANKET Blanket Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories HSC-16S-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories INCT-160 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories MMCT-75 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories TCH-165Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | >= 1600 °C | >= 2910 °F | |
China-Yixing Longly Refractories 99 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Chosun Refractories 1600HA BOARD Board Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | Intermittent |
Zircar Ceramics ZAL-45AA Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |