Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 142 °C | 288 °F | Heat Resistance; ASTM D570D |
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |