Polymer Property : Maximum Service Temperature, Air = 2851 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1566 °C
2851 °F
Recommended Operating Temperature
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator
Fibermax Mat is a high-temperature, flexible mat product that is lightweight (1.5 lb/ft3 density) and highly resilient. It is composed entirely of Fibermax polycrystalline mullite fibers to produce..
Maximum Service Temperature, Air 1566 °C
2851 °F
Recommended Operating Temperature
Unifrax Fiberfrax® Fiberstick™ Cement Refractory Cement
Fiberstick™ refractory cement is a high-temperature, air-setting mortar used as an adhesive to securrely bond Fiberfrax bonded modules and other product forms to refractory surfaces.Typical Applica..