Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1500 °C | 2732 °F | |
Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95% This ultra high temperature yttrium oxide coating provides exceptional protection of graphite, ceramic and metal components exposed to reactive molten metals such as titanium, uranium and their allo.. |