Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 97.2 °C | 207 °F | Heat Distortion, Annealed; ASTM D648 |
Total 680 Polystyrene
(discontinued **) Polystyrene 680 is a medium impact polystyrene developed for the foam extrusion and laminate markets. This polymers impact qualities in conjunction with its high flexural strength allow 680 to be ex.. |
|||
Maximum Service Temperature, Air | 97.0 - 110 °C | 207 - 230 °F | Softening Range |
Huntsman Araldite GT 7074 Bisphenol A Epoxy Solid Resin Weight per Epoxide (EEW, g/eq) 935 to 1175. Max color is 2.Comments/Applications: Unmodified bis A "Type 4+" epoxy. Medium melt viscosity epoxy for thick film powder coatings. Outstanding adhesio.. |
|||
Maximum Service Temperature, Air | 97.0 °C | 207 °F | Heat Distortion Temp |
Hannam Chemical Hanalac H-2938 ABS |
|||
Maximum Service Temperature, Air | 97.2 °C | 207 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSC 523 Polystyrene Polystyrene 523 is a high flow, high heat crystal. Specially designed for foam applications it has a very narrow molecular weight distribution. Performance in extruded loose fill foam is excellent d.. |
|||
Maximum Service Temperature, Air | 97.0 °C | 207 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B3S BK00464 PA6 (Conditioned) Description: Easy flowing, finely crystalline injection-molding grade for very fast processing. Uses include thin-walled technical parts (eg. housings, fittings, grips, small parts and fixing clamps.. |
|||
Maximum Service Temperature, Air | 97.0 °C | 207 °F | for 50% loss of tensile strength after 5,000 hr |
BASF Ultramid® B3S BK00464 PA6 (Dry) Ultramid B3S BK00464 is an easy flowing, pigmented black, finely crystalline injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Maximum Service Temperature, Air | 97.0 °C | 207 °F | for 50% loss of tensile strength after 5,000 hr |
BASF Ultramid® B3S HP PA6 (Conditioned) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |
|||
Maximum Service Temperature, Air | 97.0 °C | 207 °F | for 50% loss of tensile strength after 5,000 hr |
BASF Ultramid® B3S HP PA6 (Dry) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |