Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 90.0 °C | 194 °F | UL 746 ABC |
Plaskolite Optix® CA-75 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Short Term |
Murtfeldt Material ”S”® 1000 Green Polyethylene Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | UL 746 ABC |
Plaskolite West Optix® CA-80 General Purpose Acrylic Resin Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable 1802-xx05FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable JLK51L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL A63 SG15 Nylon 6.6 for injection molding, 15% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
Lehmann & Voss LUVOCOM® 6/CF/30 Polyamide 12, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
Lehmann & Voss LUVOCOM® 6-8548 Polyamide 12, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
Lehmann & Voss LUVOCOM® G Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
LATI Laticonther 62 CPG/750 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 65014 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
Trelleborg Emerson & Cuming Eccobond® 15 Variable Hardness Catalyst Emerson & Cuming 15 Eccobond® Variable Hardness CatalystEasy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener used. Long working life. Yields cured .. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30 Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® BG-40 S PA6-GF40 Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 20 LF grey PA12 Product Description: Grilamid L 20 LF grey is a medium viscosity graphite filled Polyamide 12 (PA12) grade suitable for both injection molding and extrusion applications. Grilamid L 20 LF grey has b.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 25 NZ ESD PA12 Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of .. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30 Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® LV-65H SST black 9288 PA12-GF65 Product description: Grilamid LV-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the f.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® LVX-50H black 9230 PA12-GF50 Product description: Grilamid LVX-50H black 9230 is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65 Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | short term; EMS |
EMS-Grivory Grivory® TR XE 4010 PA*-I Product description: Grilamid XE 4010 is an amorphous cycloaliphatic copolyamide based on 58 % renewable resources. The material is designed for applications where high chemical resistance, high fat.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® TSG-50 PA666-GF50 Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® LBV-65H FWA nat PA12-GF65 Product description: Grilamid LBV-65H FWA natural is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® LKN-3H PA12-GB30 Product description: Grilamid LKN-3H is a 30% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
3M PN8019 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
Styrolution Luran® S KR 2867 C WU Colored ASA+PC Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.Information provided by STYROLUTION, which is a joint venture between BASF and INEO.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® BM-30/2 PA6-MD30 Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50 Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |