Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 982 °C | 1800 °F | Continuous |
Pyrotek I-28 Insulating Board Pyrotek's I-28 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-28 also contains no RCF's.A.. |
|||
Maximum Service Temperature, Air | 980 °C | 1800 °F | Continuous |
Pyrotek N-20T Compressible Insulation Board Excellent characteristics allow for the manufacture of a very durable, smooth, hard roll surface which is non-marking to glass. Works well when a high temperature compressible gasket is required.Ap.. |
|||
Maximum Service Temperature, Air | 980 °C | 1800 °F | |
GBC Cerasilâ„¢ 223U Ceramic Has a lower CTE, better thermal shock resistance, lower firing temperature, and lower consistent shrinkage than steatite.Applications: ideal for volume production of small pressed insulators often r.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | |
Meehanite HS Heat Resisting Cast Iron Type HS compares very favorably from a strength standpoint with any heat resisting metal. Compositional adjustments are made to suit the exact service conditions. It machines easily and provides m.. |
|||
Maximum Service Temperature, Air | 980 °C | 1800 °F | |
MetalTek MTEK 20-25 Cast UNS J94213 Heat Resistant Stainless Steel Provides strength levels of HT with better ductility.Applications: Furnace skids for slabs, bars, furnace fixturesInformation provided by MetalTek |
|||
Maximum Service Temperature, Air | 980 °C | 1800 °F | |
MetalTek MTEK 35-15 Cast UNS N08605 Heat Resistant Stainless Steel Good strength at heat treating temperatures. Resists thermal shock of repeated heating and cooling.Applications: Dampers, pots, blades, rolls, door frames, retorts, rolling mill guides.Information p.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Continuous |
Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat CERMEX® MT1800 Needled Silica Blanket is a binderless material comprised of high purity, amorphous silica fibers. In demanding applications, the abrasion and vibration resistance of this mat make.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Continuous |
Mid-Mountain Materials SILTEX® 1800 Amorphous Silica Industrial Textile SILTEX® 1800 is a family of high performance textiles comprised of high purity, high strength amorphous silica fibers. SILTEX® 1800 Industrial Textiles demonstrate excellent thermal stability,.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Continuous |
Mid-Mountain Materials SILTEX® 36 Amorphous Silica Textile Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use wher.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Upper limit of working range |
Heatbath/Park No-Carb 1397 Stop-Off/Protective Coating for Steel A new, water-washable, stop-off compound for gas, vacuum or pack carburizing. Effective stop-off for case depths to .250" at temperatures as high as 1800°FInformation provided by Heatbath Corpor.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Vari-Form™ A Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Vari-Form™ B Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Continuous |
Unifrax Foamfrax® Isofoam® RG Insulation Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory.. |
|||
Maximum Service Temperature, Air | 980 °C | 1800 °F | Te Value Tk1 |
Advanced Ceramics ALC 1082 (C-786) Alumina Information provided by Advanced Ceramics Limited (ACL) |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | oxidation resistance to this temp |
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Sheet and Strip, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | |
BNZ Materials 508 Insulating Cement 508 Insulating Cement is an 1800°F service product, utilized in the refractory applications requiring a combination of insulating value and high temperature performance. Typical Applications: Insul.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | oxidation resistance to this temp |
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Plate, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Intermittent |
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286 Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at .. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Scaling Temperature for Continuous Service |
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Scaling Temperature for Continuous Service |
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |