Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 77.0 °C | 171 °F | Deflection temperature; load unknown. |
Abatron AboCast 8-12/Abocure 8-12 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/13.2 ratio (pbw); Gel time, 100 g (3.5 oz.): 49 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F.. |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | Deflection temperature; load unknown. |
Abatron AboCast 8-13/Abocure 8-13 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 53 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°.. |
|||
Maximum Service Temperature, Air | 77.0 - 87.0 °C | 171 - 189 °F | Softening Range |
Huntsman Tactix XP 71756.00 Epoxy Weight per Epoxide (EEW, g/eq) 245 to 265.Comments/Applications: Dicyclopentadiene based epoxy. Functionality 3.2.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquire.. |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | Heat Distortion Temp |
Hannam Chemical Hanalac 795 ABS, Pipe Grade Designed for pipe and bobbin sleeves. Excellent processability and high impact strength. Manufactured to prevent static electricity. |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | Heat Distortion Temp |
Hannam Chemical Hanalac HFA-700 ABS |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | |
ChevronTexaco Delo® NLGI 00 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | |
ChevronTexaco Dura-Lith® NLGI 00 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Maximum Service Temperature, Air | 77.2 °C | 171 °F | |
Bostik 6332 Quick Setup EVA Glue Stick Bostik 6332 Quick Setup EVA Glue StickShort open time and quick set up. Low viscosity. Easy to gun. Withstands elevated temperatures. |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | |
3M 471 Vinyl Tape 3M™ Vinyl Tape 471 is a conformable colored (9 colors plus transparent) tapes made from vinyl backing with rubber adhesive. They are ideal for many lane and safety markings, color coding, abrasion .. |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | |
3M 4712 Vinyl Tape 3M™ Vinyl Tape 4712 is a conformable colored (9 colors plus transparent) tapes made from vinyl backing with rubber adhesive. They are ideal for many lane and safety markings, color coding, abrasion.. |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | |
3M 5700 Safety Stripe Tape 3M™ Safety Stripe Tapes are durable vinyl tapes used to identify and mark traffic areas and physical hazards.Information provided by 3M |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | |
3M 5702 Safety Stripe Tape 3M™ Safety Stripe Tapes are durable vinyl tapes used to identify and mark traffic areas and physical hazards.Information provided by 3M |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | Service |
3M 7710 Acetate Identification Label Material 3M™ Label Material 7710 gloss clear acetate with 3M™ 400 high tack acrylic adhesive offers consistent, high quality appearance and excellent UV resistance. The transparent film easily die-cuts whi.. |
|||
Maximum Service Temperature, Air | 77.0 °C | 171 °F | |
3M 480 Polyethylene Tape 3M™ Polyethylene Tape 480 has a transparent polyethylene backing with a long aging transparent acrylic adhesive. It can be used for splicing and repairing polyethylene sheeting. It is also recommen.. |