Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 870 °C | 1600 °F | Continuous |
Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite MM 800 (formerly MM 1600) is a compression molded glass mica composite that is the perfect alternative to high performance plastics where high temperature, good dielectric strength and good arc resi.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
ND Industries 907 Anti-seize Aluminum-Graphite Aluminum and Graphite based, general purpose lubricant |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Pyrotek PROSILY G-10R Graphite Lubricant/Coating Color - Black, Base - Graphite, Carrier - ResinApplicationsMold coating Extrusion die Dry film lubricator AdvantagesResistant to high temperature Good thermal conductivity Low coefficient of expansi.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Pyrotek PROSILY G-11R Graphite Lubricant/Coating Color - Black, Base - Graphite, Carrier - ResinApplicationsMold coating Extrusion die Dry film lubricator AdvantagesResistant to high temperature Good thermal conductivity Low coefficient of expansi.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Pyrotek PROSILY G-40W Graphite Lubricant/Coating Color - Black, Base - Graphite, Carrier - WaterApplicationsStrip caster Roll lubricator AdvantagesResistant to high temperature Good thermal conductivity Low coefficient of expansion Chemically iner.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Pyrotek Stainless Steel Mesh Core Stainless steel mesh. Flat.AdvantagesExcellent Abrasion Resistance Good Compression and Recall Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Pyrotek Steel Mesh Core Steel mesh. Tube shaped.AdvantagesExcellent Abrasion Resistance Good Compression and Recall Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning .. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
MetalTek MTEK 20-10 Cast UNS J92603 Heat Resistant Stainless Steel Economical heat resistant grade with sufficient chrome and nickel for good oxidation resistance.Applications: Burner tips, furnace rails, annealing boxes, trays, burnishing rolls.Information provide.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Lucas-Milhaupt Dry Flux Silver Brazing Flux Dry Flux is a premium quality brazing flux in powdered form consisting of a unique combination of borates and fluorides for use with torch, induction, furnace, resistance, dip and other heating meth.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Lucas-Milhaupt Ultra Flux Silver Brazing Flux Ultra Flux is a water base paste consisting of a unique combination of potassium salts of fluorine and boric acid. It is recommended for use with torch, induction, furnace, resistance, dip and other.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | oxidation resistance, intermittent |
H.C. Starck Ampersint® AISI 316 L 300 µm For P/M, HIP/CIP, MIM AISI 316 L is a type of low carbon austenitic Cr-Ni-Mo stainless steel with good oxidation resistance in intermittent service to 870°C and in continuous service to 925°C, resistance to intercr.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | oxidation resistance, intermittent |
H.C. Starck Amperweld® AISI 316 L 150/53 µm for Plasma Transferred Arc Surfacing AISI 316 L is a type of low carbon austenitic Cr-Ni-Mo stainless steel with good oxidation resistance in intermittent service to 870°C and in continuous service to 925°C, resistance to intercr.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | long continuous heating |
Meehanite HSV Heat Resisting Cast Iron Type HSV is an iron developed essentially for engineering parts subjected to long continuous heating. It has been designed to have the maximum load bearing ability.General Meehanite information - M.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | oxidation resistance, intermittent |
H.C. Starck Ampersint® AISI 316 L 31 µm For P/M, HIP/CIP, MIM AISI 316 L is a type of low carbon austenitic Cr-Ni-Mo stainless steel with good oxidation resistance in intermittent service to 870°C and in continuous service to 925°C, resistance to intercr.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Lucas-Milhaupt Dispensable Flux Dispensable Flux is a water base consisting of a unique combination of potassium salts of fluorine and boric acid. It is recommended for use with torch, induction, furnace, resistance, dip and other.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Universal Wire Works 347 Stainless Steel Electrode Universal 347 electrodes were developed for the welding of types 321 and 347 stainless and the clad side of steel clad with like alloys. Alloy 347 is used for the fabrication of equipment, which mus.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Universal Wire Works 430 Stainless Steel Electrode Universal 430 electrode deposits contain approximately 16% chromium in a carefully balanced composition to provide outstanding resistance at temperatures up to 1600 degrees F. Deposits are martensit.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
XADC-Armoloy Armoloy® TDC Hard Chromium Coating ARMOLOY® TDC is a low temperature, multi-state surface finishing process. ARMOLOY® utilizes proprietary chemical solutions and application processes that are carefully monitored to produce it.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
BNZ Materials 460 Insulating Cement 460 Insulating Cement is a 1600°F product, provided in higher density than 508 Insulating Cement. 460 Cement can be applied in heavy layers. It is frequently used as the principal covering on pipe .. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Aremco Pyro-Putty™ 2500 High Temperature Ceramic-Metallic Putty, Iron Oxide Filled Ceramic and Black Iron Oxide-Filled, One-Part, Water Based Paste.For Applications to 1/4" Thick.Repairs Cast Iron, and Steel Parts to 1600°F |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | Continuous |
Aremco Quartz-Coat™ 850 High Temperature Specialty Coatings Inorganic, Glass-Ceramic Filled Glass-ceramic, white reflective coating for glass and quartz to 1500°F (816°F) |