Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Neoprene Version |
Parker Chomerics COMBO® Gaskets Wire Mesh EMI Gasket Selection Guide Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Die-Cut Elastomer with Joined EMI Strips.Standard Metals Available in EMI Portion: Mone.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Wet Service |
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Continuous (Water Immersion) |
Chesterton ARC 791 Composite Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | for 30 mins |
3M 101+ Value Masking Tape 3M™ Value Masking Tape 101+ is a tan colored crepe paper masking tape for holding, bundling, sealing, and non-critical masking applications where a pressure sensitive tape is needed.Information pro.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | for 30 mins |
3M 2209 Paper Masking Tape 3M™ Paper Masking Tape 2209 is an economy crepe paper tape for holding, bundling, sealing, and non-critical masking jobs where a pressure sensitive tape is needed.Information provided by 3M |
|||
Maximum Service Temperature, Air | 66.1 °C | 151 °F | |
Bostik 6328 Low Viscosity, Long Open Time, Flexible EVA Glue Stick Bostik 6328 Low Viscosity, Long Open Time, Flexible EVA Glue StickLow viscosity. Easy to gun. Long open time. Flexible, no cracking. Excellent bonding range. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | |
3M 4714 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Short Term |
3M 9824 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Short Term |
3M 9828PC Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M Bumpon™ SJ5208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M Bumpon™ SJ5216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M SJ5400 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M SJ6100 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Deflection Temp at unknown load |
Abatron AboCast 7703-21/AboCure 7703-23 (C) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | |
3M 4314 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M Bumpon™ SJ6208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | |
3M Safety-Walk™ 280 White Slip-Resistant Fine Resilient Tapes and Treads A fine-textured, slip-resistant surface with a pressure-sensitive adhesive backing provides enhanced safety and comfort in light- and barefoot- traffic areas. For wet, barefoot-traffic areasNon-mine.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | |
3M 4718 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | |
3M 4726 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Service |
3M Bumpon™ SJ5808 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 66.0 °C | 151 °F | Wet |
Chesterton MRS 10 Metal Rebuilding System Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance It is non-sagging, non-shrinking and 10.. |