Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 55.0 °C | 131 °F | |
Abatron 416 A/B Filled Potting Compound
(discontinued **) Phosphorescent litegreen resin. 100/26 ratio.Information provided by Abatron. |
|||
Maximum Service Temperature, Air | 55.0 °C | 131 °F | |
LATI Latamid 6 E02 PA 6, Impact modified Polyamide 6 (PA6). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A... |
|||
Maximum Service Temperature, Air | 55.0 °C | 131 °F | as heat transfer fluid |
Solvay Specialty Polymers Galden® HT55 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Maximum Service Temperature, Air | 55.0 °C | 131 °F | Continuous |
Wolf Kunststoff ZEDEX® ZX-100A Polymer Alloy Main Characteristics: Tough; Resilient; Soft; Low cost solutionApplications: Handling, Vessel and pump, Steel and Water, Chemical Engineering, Automitve Technology, Machine ToolsInformation provided.. |
|||
Maximum Service Temperature, Air | 55.0 °C | 131 °F | Deflection temperature; load unknown. |
Abatron AboCast/AboCure 8109-3 Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140.. |
|||
Maximum Service Temperature, Air | 55.0 °C | 131 °F | Deflection temperature; load unknown. |
Abatron AboCast/AboCure 8109-4 Safety hardener (minimum toxicity) version of 8109-3.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 .. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 007 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 019 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 022 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 025 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 027 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 029 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 032 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 036 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 042 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 047 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 049 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 057 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 089 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 3273 Standard SBS Thermoplastic Elastomer Compound |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 3275 Standard SBS Thermoplastic Elastomer Compound |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 3276 Standard SBS Thermoplastic Elastomer Compound |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 003 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 068 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 075 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 076 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 081 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 084 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
AlphaGary Evoprene™ 091 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |