Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park AL-2 for Aluminum Solution Heat Treating A granular mixture of sodium and potassium nitrates formulated per MIL-H-6088. It is less costly than Tempering C-ALHT with only a slight sacrifice in working range. It is colored pink for identif.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Aus-Quench Quenching and Tempering Salt Quench salt whose melting point and working range make it particularly suitable for ausquenching/austempering. (350 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Low Temperature Draw Salt Quenching and Tempering Salt A eutectic mixture offering the lowest melting point and a wide working range. Formulated per MIL-S-10699-B, Class 1 (275 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical... |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Parcure 290 Rubber Cure Salt Nitrate/Nitrite Salt. An eutectic mixture with slightly higher melting point and narrower working range but lower in cost than Parcure 275. (290 Parkettes)Information provided by Heatbath Corporati.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Partherm 430 Heat Transfer Salt A popular heat transfer salt for use in the higher temperature ranges. It is more inert to ferrous alloys than Partherm 290 or 350 and considerably lower in cost. Its heat capacity and thermal cond.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Scale Kleen 9 Descaling Salt A highly alkaline and oxidizing salt bath for metal descaling and the removal of ceramic shell material from ferrous and nickel alloy investment castings.Information provided by Heatbath Corporation.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Parcure 275 Rubber Cure Salt Nitrate/Nitrite Salt. An eutectic mixture offering the lowest possible melting point and the widest working range. (275 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Parcure 305 Rubber Cure Salt Nitrate/Nitrite Salt. A very popular rubber cure salt that combines wide working range with low cost and relatively lower dragout when used above 400°F. (330 Parkettes)Information provided by He.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Tempering C-ALHT for Aluminum Solution Heat Treating A granular mixture of sodium and potassium nitrates formulated per MIL-S-10699-B, class 11 and MIL-H-6088. The salt is colored pink for identification purposesInformation provided by Heatbath Corpo.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | In oxygen |
SGL Carbon Group EK 204 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | In oxygen |
SGL Carbon Group V 1626 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Structural Applications |
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Operating Temperature |
California Fine Wire Nickel Alloy 99 All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco AREMCOLOX™ 502-600 Machinable Glass Ceramic High dielectric and mechanical strength. For high voltage insulators, lamp housings, thermal switches, and radiation parts. Readily machined, no firing required. Plates from 1/8" to 1" thick; rod.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone Low viscosity, green coating for power resistors to 1100°F (593°C) |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4060 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C). |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating 840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone Low viscosity, white coating for motor windings to 1100°F (593°C) |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Partherm 290 Heat Transfer Salt The most widely used heat transfer salt. It is an eutectic mixture with a low melt point and a wide working range. (290 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical. |