Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 41.0 °C | 106 °F | Long term |
3M 9925XL Extended Liner Tapes 3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p.. |