Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 400 - 550 °C | 752 - 1020 °F | High Temperature Engineering Polymers |
Claude Bamberger Ultimax® 9100 Purge Compound Ultimax® is recommended for ABS, nylon, polycarbonate, PET, and other high temperature engineering plastics. Temperature range 350-525°F (176-275°C). Ultimax® 9100 is environmentally friendlie.. |