Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 350 - 450 °C | 662 - 842 °F | Cellulosics, Polyolefins, Styrenics & PVC Resins |
Claude Bamberger Ultimax® 9100 Purge Compound Ultimax® is recommended for ABS, nylon, polycarbonate, PET, and other high temperature engineering plastics. Temperature range 350-525°F (176-275°C). Ultimax® 9100 is environmentally friendlie.. |