Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 149 - 316 °C | 300 - 600 °F | |
Neutrex Purgex™ 3056 Purging Compound Blend, polyethylene and FDA-approved active component. Non-toxic, non-abrasive, and safe. Ready to use and easy to removePURGEX 3056 Plus is used to effectively remove all types of colorants and eng.. |
|||
Maximum Service Temperature, Air | 149 - 316 °C | 300 - 600 °F | |
Neutrex Purgex™ 3057 Plus Purging Compound Blend, polyethylene, 3% glass, and FDA-approved active component. Non-toxic, non-abrasive and safe. Ready to use and easy to removePURGEX 3057 Plus thoroughly removes all types of colorants and engi.. |
|||
Maximum Service Temperature, Air | 93.3 - 316 °C | 200 - 600 °F | Average value: 260 °C Grade Count:69 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
Maximum Service Temperature, Air | 230 - 316 °C | 446 - 601 °F | Average value: 263 °C Grade Count:42 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |