Polymer Property : Maximum Service Temperature, Air = 288 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 138 - 288 °C
280 - 550 °F
Neutrex Purgex™ 456 Plus Purging Compound
Blend, polyethylene, and FDA-approved active component. Non-toxic, non-abrasive, and safe. Ready to use and easy to remove.PURGEX 456 Plus is used for color and/or material changes and the removal o..
Maximum Service Temperature, Air 149 - 288 °C
300 - 550 °F
Neutrex Purgex™ 457 Purging Compound
Blend, polyethylene, 3% glass, and an FDA-approved active component. Non-toxic, non-abrasive, and safe. Ready to use and easy to removePURGEX 457 Plus is used for color and/or material changes and t..
Maximum Service Temperature, Air 204 - 288 °C
400 - 550 °F
High Temperature Engineering Plastics
Claude Bamberger Bamberko® 9016 Purge Compound
Bamberko® is recommended for cellulosics, polyolefins, styrenics, and PVC resins. Temperature range 350-525°F (176-275°C). Formulated to flow through injection cylinders and extrusion barrels w..