Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 150 - 250 °C | 302 - 482 °F | Average value: 211 °C Grade Count:12 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Maximum Service Temperature, Air | 90.0 - 250 °C | 194 - 482 °F | Average value: 133 °C Grade Count:15 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Maximum Service Temperature, Air | 90.0 - 250 °C | 194 - 482 °F | Average value: 164 °C Grade Count:24 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Maximum Service Temperature, Air | 90.0 - 250 °C | 194 - 482 °F | Average value: 164 °C Grade Count:23 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Maximum Service Temperature, Air | 135 - 250 °C | 275 - 482 °F | Average value: 186 °C Grade Count:6 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Maximum Service Temperature, Air | 110 - 250 °C | 230 - 482 °F | Average value: 160 °C Grade Count:3 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Maximum Service Temperature, Air | 80.0 - 250 °C | 176 - 482 °F | Average value: 140 °C Grade Count:6 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Maximum Service Temperature, Air | 230 - 250 °C | 446 - 482 °F | Softening Range |
Huntsman DT 3355 Matting Agent Color: Off-whiteComments/Applications: Reactive matting agent for low gloss epoxy and epoxy/polyester hybrid powder formulations.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals ha.. |
|||
Maximum Service Temperature, Air | 150 - 250 °C | 302 - 482 °F | Average value: 184 °C Grade Count:5 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Maximum Service Temperature, Air | 130 - 250 °C | 266 - 482 °F | Average value: 163 °C Grade Count:8 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Maximum Service Temperature, Air | 93.0 - 250 °C | 199 - 482 °F | Average value: 178 °C Grade Count:6 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |