Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 75.0 - 210 °C | 167 - 410 °F | Average value: 151 °C Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Maximum Service Temperature, Air | 188 - 210 °C | 370 - 410 °F | Average value: 200 °C Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Maximum Service Temperature, Air | 108 - 210 °C | 226 - 410 °F | Average value: 145 °C Grade Count:10 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |