Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | Long Term |
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer
(Unverified Data**) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | Long Term |
Kolon Kocetal® CL704 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long time operation |
Zell-Metall Engineering Plastics Zellamid 1100 Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long time operation |
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long time operation |
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Maximum Service Temperature, Air | 80.0 - 120 °C | 176 - 248 °F | |
Goodfellow Cobalt/Silicon/Boron/Manganese Alloy Information provided by Goodfellow.Composition Notes: Si + B content = 25 wt%. Fe+Mo content = 2 wt%. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® AG-35 PA66-GF35 Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers. High stiffnessHigh tensile strengthHigh heat distortion temperatureEasy .. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® B 70 GFE 15 H PA6-GF15 Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important prop.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® BG-15/2 PA6-GF15 Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® BG-30/2 PA6-GF30 Product description: Grilon BG-30/2 is a heat stabilized, normal viscosity PA6 injection molding grade with 30% glass fibers. Grilon BG-30/2 has the following important properties: High stiffnessGoo.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® BG-40 S PA6-GF40 Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® BGZ-15 PA6-GF15 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70 Product description: Grivory GVX-7H black 9915 is a 70% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® GVX-7 H nat PA*-GF70 Product description: Grivory GVX-7H natural is a 70% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30 Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® TSG-30/4 V0 PA666-GF30 FR Product description: Grilon TSG-30/4 V0 is a heat stabilized, flame retardant, self-extinguishing engineering thermoplastic, reinforced with glass-fiber 30% (by weight) based on a semi-crystalline P.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® TSG-50 PA666-GF50 Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® XE 4107 black 9992 PA612-GF40 Product description: Grilamid XE 4107 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorpti.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40 Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® EB 50 H DZ PA6 Product description: Grilon EB 50 H DZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon EB 50 H DZ has the following important properties:.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® GV-4H PA*-GF40 Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Maximum Service Temperature, Air | 80.0 - 120 °C | 176 - 248 °F | long term; EMS |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® LBV-65H FWA nat PA12-GF65 Product description: Grilamid LBV-65H FWA natural is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Maximum Service Temperature, Air | 110 - 120 °C | 230 - 248 °F | |
AlphaGary Evoprene™ G 991 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® BG-50 FC PA6-GF50 Product description: Grilon BG-50 FC is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50 Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |