Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 92.2 °C | 198 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSI 935E Polystyrene Polystyrene 935E is a high impact polystyrene exhibiting exceptional toughness for sheet and thermoforming applications.This polymer is an excellent choice for cups, food packaging, custom sheet and.. |
|||
Maximum Service Temperature, Air | 92.2 °C | 198 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSI 975E Polystyrene Polystyrene 975E is a high impact polystyrene designed for extrusion/thermoforming applications. The food ESCR properties of 975E dictate its use for dairy applications that are subjected to high bu.. |