Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 79.4 °C | 175 °F | Continuous |
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |
|||
Maximum Service Temperature, Air | 79.4 °C | 175 °F | Continuous |
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |
|||
Maximum Service Temperature, Air | 79.4 °C | 175 °F | |
Alcoa KAMA 2100 Prime Clear OPS, Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Maximum Service Temperature, Air | 79.4 °C | 175 °F | |
Alcoa KAMA 2200 Prime Graphic Arts OPS
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Maximum Service Temperature, Air | 79.4 °C | 175 °F | |
Alcoa KAMA 2500 Prime Clear OPS, Shrink Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Maximum Service Temperature, Air | 79.4 °C | 175 °F | |
Alcoa KAMA 2700 OPS Lamination, Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Maximum Service Temperature, Air | 79.4 °C | 175 °F | dry |
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 79.4 °C | 175 °F | |
Saint-Gobain Tygothane® C-210-A Precision Polyurethane Tubing Formulation Description: Tygothane® C-210-A: Our rigidly controlled manufacturing process makes Tygothane® Precision Polyurethane Tubing the flexible polyurethane tubing that has consistently tight toleranc.. |