Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 704 °C | 1300 °F | Upper limit of working range |
Heatbath/Park #900 High Speed Hardening Salt For quenching and tempering steel. #900 is especially suited for oil hardening followed by relatively high draw, since no washing is required between quench and draw. #900 is less hygroscopic than .. |
|||
Maximum Service Temperature, Air | 704 °C | 1300 °F | Upper limit of working range |
Heatbath/Park #900 High Speed Hardening Salt For quenching and tempering steel. #900 is especially suited for oil hardening followed by relatively high draw, since no washing is required between quench and draw. #900 is less hygroscopic than .. |
|||
Maximum Service Temperature, Air | 704 °C | 1300 °F | Upper limit of working range |
Heatbath/Park #900 Neutral Salt For quenching and tempering steel. #900 is especially suited for oil hardening followed by relatively high draw, since no washing is required between quench and draw. #900 is less hygroscopic than .. |
|||
Maximum Service Temperature, Air | 704 °C | 1300 °F | Upper limit of working range |
Heatbath/Park #900 Quenching and Tempering Salt For quenching and tempering steel. #900 is especially suited for oil hardening followed by relatively high draw, since no washing is required between quench and draw. #900 is less hygroscopic than .. |
|||
Maximum Service Temperature, Air | 704 °C | 1300 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® 440 Ceramic Fiber Paper 440 paper is a low-cost, high-strength composite paper made from a combination of ceramic fiber, inert fillers, and reinforcing fiberglass. The fiberglass gives added strength to the 440 paper at o.. |
|||
Maximum Service Temperature, Air | 704 °C | 1300 °F | Continuous use |
Pyrotek E-1 Board Structural Insulating Board E-1 is a high-temperature board designed to combine structural strength and high insulating value. Structural insulation panels made from E-1 can be painted. Fibers generated while cutting E-1 are .. |