Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park AL-2 for Aluminum Solution Heat Treating A granular mixture of sodium and potassium nitrates formulated per MIL-H-6088. It is less costly than Tempering C-ALHT with only a slight sacrifice in working range. It is colored pink for identif.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park AL-2 High Speed Hardening Salt A mixture of nitrates in granular form especially formulated as an economical bath for tempering tool steels requiring treatment within its working range. This highly fluid bath offers low dragout b.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park AL-2 Quenching and Tempering Salt A mixture of nitrates in granular form especially formulated as an economical bath for tempering tool steels requiring treatment within its working range. This highly fluid bath offers low dragout b.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park High Temp Draw Salt Quenching and Tempering Salt Salt mixture particularly suitable for ausquenching/austempering. (430 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Marquench Quenching and Tempering Salt Low cost quench salt with slightly higher melting point and narrower working range than Low Temp Draw Salt and Thermo-Quench salts. It is as fluid as lower melting salts above 400°F offering equi.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Parcure 290 Rubber Cure Salt Nitrate/Nitrite Salt. An eutectic mixture with slightly higher melting point and narrower working range but lower in cost than Parcure 275. (290 Parkettes)Information provided by Heatbath Corporati.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Parcure 300 Rubber Cure Salt A nitrite-free alternative for customers concerned with the introduction of nitrosamines from the alkali nitrite raw materials used in the production of commercial rubber cure salts. Within its work.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Partherm 430 Heat Transfer Salt A popular heat transfer salt for use in the higher temperature ranges. It is more inert to ferrous alloys than Partherm 290 or 350 and considerably lower in cost. Its heat capacity and thermal cond.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Scale Kleen 9 Descaling Salt A highly alkaline and oxidizing salt bath for metal descaling and the removal of ceramic shell material from ferrous and nickel alloy investment castings.Information provided by Heatbath Corporation.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Thermo-Quench Quenching and Tempering Salt Most widely used quench salt for more than a decade. This eutectic nitrate/nitrite mixture is highly recommended for the interrupted or isothermal quenching of austenitized steels. Slightly higher,.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Parcure 305 Rubber Cure Salt Nitrate/Nitrite Salt. A very popular rubber cure salt that combines wide working range with low cost and relatively lower dragout when used above 400°F. (330 Parkettes)Information provided by He.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | In oxygen |
SGL Carbon Group EK 204 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | In oxygen |
SGL Carbon Group V 1626 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Structural Applications |
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Operating Temperature |
California Fine Wire Copper, 27% Nickel Clad All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Operating Temperature |
California Fine Wire Nickel Alloy 99 All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4060 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C). |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating 840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone Low viscosity, white coating for motor windings to 1100°F (593°C) |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | |
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Continuous |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Maximum Service Temperature, Air | 593 °C | 1100 °F | Upper limit of working range |
Heatbath/Park Partherm 290 Heat Transfer Salt The most widely used heat transfer salt. It is an eutectic mixture with a low melt point and a wide working range. (290 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical. |