Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 43.3 °C | 110 °F | Upper limit of working range |
Heatbath/Park Plastiquench Water-Based Quenchant A solution of polyvinyl alcohol in water, used as a base for steel quenching media. In water solution, it cools austenitized steels faster then quenching oils, hardens steels with less distortion or.. |