Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application Temp |
Chesterton 775 Moisture Shield Description: Chesterton® 775 Moisture Shield is a moisture displacing, clear protective coating that protects parts and equipment from corrosion for months. Sprayed on bare metal, it leaves a lubri.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FM0186N Clear Polyester Label Products 3M™ Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FM023402 Clear Polyester Label Products 3M™ Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FM1542 Clear Polyester Label Products 3M™ Clear Polyester Label Products FM1541 and FM1542 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesi.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP0122R2 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP016902 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP017102 White Polyester Label Products 3M™ White Polypropylene Label Products FP017102 and FP026508 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general purpose permane.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP019802 White Polyester Label Products 3M™ White Polypropylene Label Products FP019802 and FP019808 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is for labeling tires when u.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP024408 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products FP024402 and FP024408 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra remova.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP024502 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra removable acrylic designed t.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP024900 White Polypropylene Label Products 3M™ White Polypropylene Label Products are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP031105 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FV053 Tire Vinyl Label Products 3M™ Tire Vinyl Label Products are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling tires when used w.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FV055 Tire Vinyl Label Products 3M™ Tire Vinyl Label Products are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling tires when used w.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FV1222R Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FV1225 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FV855 Tire Vinyl Label Products 3M™ Tire Vinyl Label Products FV852 and FV855 are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling t.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M PS191 White Yupo™ TIS Label Products 3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M PS193 White Yupo™ TIS Label Products 3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FM1541 Clear Polyester Label Products 3M™ Clear Polyester Label Products FM1541 and FM1542 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesi.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP024503 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra removable acrylic designed t.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP02450N Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra removable acrylic designed t.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FP024902 White Polypropylene Label Products 3M™ White Polypropylene Label Products are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FV010002 Removable Vinyl Label Product 3M™ Removable Vinyl Label Product FV010002 is a flexible, conformable white vinyl label stock that offers durability and moisture resistance. This vinyl label utilizes 3M™ Adhesive R3800, which is.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M PS102 Semi-gloss Paper Label Product 3M™ Semi-gloss Paper Label Product PS102 is a durable, general purpose paper product. This label product utilizes 3M™ Adhesive P1110, which is for labeling tires when used with tire wash. This adh.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M PS190 White Yupo™ TIS Label Products 3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FM0234R2 Clear Polyester Label Products 3M™ Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FV016405 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FV0164R2 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |
|||
Maximum Service Temperature, Air | 43.0 °C | 109 °F | Application |
3M FV016408 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |