Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 400 °C | 752 °F | Continuous |
Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Better radiation resistance (3 x 10^10 Rads-Cobalt) than grade 400.This ceramoplastic material is a versatile and efficient insulating material designed to me.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
P & P Technology Silver/Aluminum Conductive Adhesive P & P Technology conductive silver/aluminum adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exp.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
GrafTech eGRAF® SPREADERSHIELD™ SS300 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
GrafTech GRAFOIL® GHN Standard Fluid Sealing Laminate, Non-Metal Reinforced GRAFOIL® Grade GHN is an unbranded laminate made with GRAFOIL® Grade TG-337 flexible graphite, thermally bonded to both faces of a plastic insert. It is not certified to any industry standards.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
GrafTech eGRAF® HITHERM™ HT-1220 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | 0.030", 0.060", 0.062", 0.082" thick |
GrafTech GRAFOIL® GRAFKOTE® Laminates, Non-Metal Reinforced GRAFOIL® GRAFKOTE® laminates are made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0005" thick polymer facing on one ("Single-Sided") or both ("Double-Sided") sides. Th.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | oxidation limit |
Momentive Performance Materials Pyrolytic Graphite (PG) Coating PG is a popular coating for sealing machined graphite hardware which does not require oxidation protection. It is the most anisotropic commercially available material and is therefore useful where .. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
Goodfellow TZM Molybdenum High Temperature Alloy Increased high temperature strength over pure molybdenum although, like Molybdenum, it oxidizes rapidly in oxidizing atmospheres above 500°CInformation provided by Goodfellow. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 100A Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 100KN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 100VN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 300A Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 300FPC Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 300KN Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 500FPC Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thic.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 50EN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 50FPC Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 50VN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 50ZT Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Intermittent |
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 100FPC Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Maximum Service Temperature, Air | 400 °C | 752 °F | Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F). |
DuPont™ Kapton® 200HN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General .. |