Polymer Property : Maximum Service Temperature, Air = 324 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 324 °C
615 °F
Greene Tweed CHEMRAZ® 615 Perfluoroelastomer
Greene Tweed’s Chemraz® 615 exhibits outstanding high temperature properties, with a temperature range from 0°F to 615°F (-18°C to 324°C). Chemraz 615’s chemical resistance..
Maximum Service Temperature, Air 324 °C
615 °F
Greene Tweed CHEMRAZ® 618 Perfluoroelastomer
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r..
Maximum Service Temperature, Air 324 °C
615 °F
Greene Tweed CHEMRAZ® 653 Perfluoroelastomer
Chemraz® is a black perfluoroelastomer specifically formulated to meet the extreme demands of diffusion, LPCVD and thin dry processing applications. It exhibits superior compression set resistan..