Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 316 °C | 600 °F | Film Temperature |
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | optimum use range |
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid Paratherm HE® is a high flash and fire point heat transfer fluid. Engineered for higher thermal and oxidative stability, it is efficient and cost effective. Its greater purity allows it to strong.. |
|||
Maximum Service Temperature, Air | <= 316 °C | <= 600 °F | max. recommended film temperature |
Paratherm Corporation Paratherm™ MR Heat Transfer Fluid Description: Paratherm MR® is a mid-range heat transfer fluid. It is efficient across the temperature range, thermally stable and cost-effective. Non-aromatic and non-toxic, the fluid is safe to .. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Intermittent |
Dielectric Polymers NT-590 Polyimide Film Tape
(discontinued **) Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized class 392°FHigh temperature resistantClean tape removalApplications: For high temperature masking, protecting gol.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Long Term |
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet) Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI .. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Greene Tweed CHEMRAZ® 555 Perfluoroelastomer With its broad chemical resistance, Chemraz® 555, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. Chemraz 555 provides a significantly wider operational band.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Greene Tweed CHEMRAZ® 655 Perfluoroelastomer Chemraz® 655 is Greene Tweed’s high-temperature off-white perfluoroelastomer. Specifically developed for wafer processes with operating temperatures up to 315°C (600°F), Chemraz 655 p.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Short Term |
Mid-Mountain Materials HYTEX® 400 Kevlar® Industrial Textile Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemi.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® 30 Brazing Alloy Silvaloy 30 is historically a modification of Silvaloy 35 with further reduction in silver content resulting in a higher melting point and a longer range. Silvaloy 30 is used for brazing steel, stai.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy Silvaloy 45 is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining s.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A38T Brazing Alloy Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A56T Flux Coated Rod Brazing Alloy Silvaloy A56T Flux Coated Rod has the lowest brazing temperature, best wetting, and best flow of all the cadmium free alloys. It has a slight plastic range which may be noticed during melting on som.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy Silvaloy is one of the lower melting brazing alloys composed of silver, copper, zinc and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, s.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® 50N Brazing Alloy Silvaloy 50N is a modification of Silvaloy 50. It was originally introduced because of somewhat better corrosion resistance than Silvaloy 50 for certain conditions, and is still used for such purpos.. |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | |
Saint-Gobain Fluoroloy® A15 High Performance Seal Material Improved sealing at low pressure; Can be abrasive running against soft metals
Information provided by Saint-Gobain Performance Plastics. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | UL-746 B |
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Cotronics 4700 Ultra Temp Adhesive and Casting Epoxy, General Purpose |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | |
3M 363LC High Temperature Aluminum Foil/Glass Cloth Tape 3M™ High Temperature Aluminum Foil/Glass Cloth Tape 363LC can be used as a high temperature, heat reflective, protective wrap for certain cables and other components in aerospace and industrial app.. |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | |
3M 433 Premium Performance Aluminum Foil Tape Silicone adhesive for high temperature resistance; MIL-T-47014, FAR 25.853, UL 746C Recognized; smooth easy unwind; clean, straight edges with minimal wrinkling.Information provided by 3M |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | Operating Temperature |
California Fine Wire Stablohm 800 Nickel, Chromium, Aluminum, and Copper Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4010S High Temperature Protective Coating Silicone-Polyester |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Maximum Service Temperature, Air | 316 °C | 601 °F | Ductility loss due to carbon phase precipitation above this temp. |
ATI Allegheny Ludlum AL 200™ Nickel Alloy, UNS N02200 Ferromagnetic. Allegheny Ludlum AL 200 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Aremco-Seal™ 529HV High Temperature Specialty Coatings Silicone High viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
Maximum Service Temperature, Air | >= 316 °C | >= 600 °F | UL-746 B |
Saint-Gobain Meldin® 2021 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |