Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 288 °C | 550 °F | Constant |
Plasma Coatings 200-HT Surface Material Information provided by Plasma Coatings |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | optimum use range |
Paratherm Corporation Paratherm™ MR Heat Transfer Fluid Description: Paratherm MR® is a mid-range heat transfer fluid. It is efficient across the temperature range, thermally stable and cost-effective. Non-aromatic and non-toxic, the fluid is safe to .. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Technetics Group PLASTOLON™ PTFE Outdoor Fiber
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Technetics Group PLASTOLON™ PTFE Oral Care Fiber
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Manifattura Cattaneo RULON® J Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Glastic GLASTHERM HT200 Insulation Sheet HT200 features:High Hot Compressive StrengthLow Thermal ConductivityOil and Moisture ResistantReduces Heat LossHelps Control TemperatureFaster Mold StartupDesigned for reducing heat losses from plas.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Saint-Gobain Rulon® 1337 Bearing/Seal PTFE Rulon® 1337 is a tan material made entirely from FDA compliant components. It has excellent physical properties and is chemically compatible with most chemicals, except concentrated sulfuric acid.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Saint-Gobain Rulon® 1410 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Saint-Gobain Rulon® 1439 Bearing/Seal PTFE Rulon® 1439 is a white FDA compliant material that is suitable for immersed service with better wear characteristics than most other PTFE compounds. Its color makes it aesthetically pleasing for .. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Saint-Gobain Rulon® 488 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Saint-Gobain Rulon® 641 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Saint-Gobain Rulon® 945 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | Short Term |
Saint-Gobain Rulon® 954 Bearing/Seal PTFE A conductive PTFE material that is available in tape, sheet (extruded) and rod (extruded).Information provided by distributor TriStar Plastics Corp. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Saint-Gobain Rulon® F Grade Bearing/Seal PTFE F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Ru.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Saint-Gobain Rulon® XL Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 482°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | Short Term |
TriStar TriSteel PT Metal Backed PTFE Bearing System Ultraflon 602 (PT) PTFE lined metal backed bearing system, low friction, high PV, high speed sleeve, flange and thrust bearings, zero lube required, high operating temperature. Ultraflon 602 PTFE Li.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
DayGlo Gem-Tone GC-18F Emerald Green Gem-Tone® GC-18F Emerald Green is a rich, strong green colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of .. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
DayGlo GloPrill Hyperdispersed Colorant GloPrill is a high-performance fluorescent colorant developed especially for polyolefins. Designed with the plastics concentrate/masterbatch producer in mind, these supercharged colorants develop br.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | Intermittent |
3M 3615 General Purpose Glass Cloth Tape 3M™ Glass Cloth Tape 3615 is a general purpose, easy unwind tape coated with a silicone adhesive for many applications requiring high-temperature resistance, high adhesion, and a very strong, abras.. |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Technetics Group PLASTOLON™ PTFE Filtration Sewing Thread
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | |
Technetics Group PLASTOLON™ PTFE Weaving Fiber
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Maximum Service Temperature, Air | 288 °C | 550 °F | Intermittent |
Plasma Coatings 300 Surface Material Information provided by Plasma Coatings |