Thermal Properties Metric English Comments
Maximum Service Temperature, Air 209 °C
408 °F
3M Scotch-Weld™ RT40 Retaining Compound Anaerobic Adhesives
3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings..
Maximum Service Temperature, Air 209 °C
408 °F
Heat Resistance; ASTM D570D
Plenco 1581 Polyester, Briquette, Transfer Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..