Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1150 °C | 2100 °F | Dry Air |
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | Dry Air |
Outokumpu 4762 High Temperature Ferritic Stainless Steel Highest chromium content-most resistant to reducing sulphurous gases. Susceptible to 475°C embrittlement and s-phase forms during long exposures in the range 600-800°C.Applications: Mostly used i.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | |
Pyrotek AL-THERM 2100H Vacuum formed refractories for use with modular hot top systems Pyrotek offers a variety of vacuum formed products composed from Al-Therm 2100H. These alumina-silicate fibers feature a unique inorganic binder system and are custom designed to shapes which are f.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | |
Gouda Vuurvast CURON 120 HS Dense Refractory Castable Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars... |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | |
MetalTek MTEK 15-65 Cast UNS N06006 Heat Resistant Stainless Steel For severe hot gas corrosion resistance at higher temperatures.Applications: Hearth plates, muffles, roller hearths, carburizing boxes.Information provided by MetalTekCast UNS N06006; Cast Grade HX;.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | Upper limit of working range |
Heatbath/Park Sta-Hard 45 High Speed Hardening Salt A stable salt for neutral heating of ferrous and nonferrous alloys. Sta-Hard45 is similar to Sta-Hard 17, but provides higher working temperatures.Information provided by Heatbath Corporation - Park.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | Upper limit of working range |
Heatbath/Park Sta-Hard 45 Neutral Salt A stable salt for neutral heating of ferrous and nonferrous alloys. Sta-Hard45 is similar to Sta-Hard 17, but provides higher working temperatures.Information provided by Heatbath Corporation - Park.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | Upper limit of working range |
Heatbath/Park Sta-Hard 45 Steel Brazing Neutral Salt A higher temperature range neutral salt used for brass or copper brazing.Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | |
Skamol Group Skamol FL-06 Insulating Mortar SKAMOL insulating mortars have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grad.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | |
Skamol Group VIP 12 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | |
CeramTec Rubalit® 600 Alumina, 48% Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors. |
|||
Maximum Service Temperature, Air | 1150 - 1250 °C | 2100 - 2280 °F | |
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy Information provided by Goodfellow. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | |
Universal Wire Works 117 Nickel Alloy Welding Wire Alloy 117 is a nickel alloy electrode for welding nickel-chromium-cobalt-molybdenum alloys (UNS # N06617). This alloy electrode provides optimum strength and oxidation resistance above 1500 degrees .. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | |
Aremco AREMCOLOX™ 502-1100 (Full-Fired) Dense Alumino-Silicate Good mechanical strength, and electrical and thermal resistance. For producing insulators, standoffs, feed-thrus, furnace carriers and brazing fixtures. Fabricate and fire yourself using conventio.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® 880 Ceramic Fiber Paper 880 paper is made from a higher alumina content, shorter, smaller diameter fiber and laid up at higher densities. These product parameters lead to reduced shrinkage, higher strength, an increased o.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® 882-H Ceramic Fiber Paper This product is completely free of organics and used when higher fired strength is required or in processes and applications where even small amounts of organic burnout is unacceptable. 882-H has h.. |
|||
Maximum Service Temperature, Air | 1150 °C | 2100 °F | |
Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |