Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1010 °C | 1850 °F | Continuous service |
ATI Allegheny Ludlum Type 441 Alloy Stainless Steel Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stab.. |
|||
Maximum Service Temperature, Air | 1010 °C | 1850 °F | Continuous service |
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy Allegheny Ludlum stainless Type AL 441HP™ alloy is a heat resisting ferritic grade providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dua.. |
|||
Maximum Service Temperature, Air | 1010 °C | 1850 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Moist Pak-D® Ceramic Fiber Insulator Fiberfrax Moist Pak-D insulation is made from high-strength ceramic fiber blankets impregnated with inorganic bonding agents. This processing results in a flexible insulation that air dries to form.. |