Polymer Property : Maximum Service Temperature, Inert = 1538 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 1538 °C
2800 °F
Retains strength
Pyrotek MC-1 Metal Ceramic Thermocouple Protection Tube
For casting, MC-1 thermocouple protection tubes are a unique blend of metal and ceramic, exhibiting properties not found solely in either individual material. MC-1 tubes offer high thermal conducti..