Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Haysite H320 Polyester Composite A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 10842N125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: Natural (Transparent)Interleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Inform.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 41300R062 0.062" Uncured Silicone Rubber on Holland Cloth Design/Construction:Interleave: 3.0 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Holland ClothThis data represents typical values for the production material and should not be used as m.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51576XC15A 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the producti.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51579XA028 0.028" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material a.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51629R020 0.020" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil polyLayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production mat.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 99410R015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate Design/Construction:Interleave: 0.001" FEPSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and sho.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon R32390B020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassAll ingredients of product are listed in 21 CFR 177.26000This data represe.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon R33073X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 7628 FiberglassSide 2: Cured Silicone RubberInterleave: NoneThis data represents typical values for the production material and should .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 30850S125 0.125" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 41580B030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 41600R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51191R014 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51224R015P 0.015" Semi-cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and shou.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51561R015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51581B015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51921R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 55359R062 62 mil Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materi.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 55503R062 0.062" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Prime Coated 162 Style FiberglassSide 2: Cured Silicone RubberThis data represents typical values for th.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon T3020-B002-## 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate 0.5 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number... |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 32580R030 0.030" Uncured Silicone Rubber on PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" PETThis data represents typical values for the production material and should not be used as mate.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 44426R010 0.010" Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Cured Silicone RubberSide 2: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassThis data represents typical values for the p.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 30850S085 0.085" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 44278R018B 0.018" Uncured/Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave 1: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 1: Cured Silicone RubberInterleave: LDPEUL R.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 48576R006 0.0055" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.0015" PolyethyleneSide 1: Uncured RubberSubstrate: Prime Coated 1080 FiberglassSide 2: Uncured RubberThis data represents typical values for the production mater.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon R37503G060 0.060" Uncured Fluorosilicone on Release PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured FluorosiliconeCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be used .. |