Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 1204 °C | 2199 °F | Reducing Atm. |
SGL Carbon Group EK 10 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 1204 °C | 2199 °F | Reducing Atm. |
SGL Carbon Group EK 17 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 1204 °C | 2199 °F | Reducing Atm. |
SGL Carbon Group EK 20 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 1204 °C | 2199 °F | Reducing Atm. |
SGL Carbon Group EK 204 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 1204 °C | 2199 °F | Reducing Atm. |
SGL Carbon Group EK 24 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 1204 °C | 2199 °F | Reducing Atm. |
SGL Carbon Group V 1626 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |