| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Pyrotek MC-1 Metal Ceramic Thermocouple Protection Tube
For casting, MC-1 thermocouple protection tubes are a unique blend of metal and ceramic, exhibiting properties not found solely in either individual material. MC-1 tubes offer high thermal conducti..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 715 Copper Nickel 30%, 1/2 Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 715 Copper Nickel 30%, 1/4 Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 715 Copper Nickel 30%, Annealed
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 715 Copper Nickel 30%, Extra Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 715 Copper Nickel 30%, Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 715 Copper Nickel 30%, Spring
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 770 Nickel Silver 18%, 1/2 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 770 Nickel Silver 18%, 1/4 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 770 Nickel Silver 18%, 3/4 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 770 Nickel Silver 18%, Annealed
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 770 Nickel Silver 18%, Extra Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 770 Nickel Silver 18%, Extra Spring
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 770 Nickel Silver 18%, Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
|
|||
| Thermal Conductivity | 29.4 W/m-K | 204 BTU-in/hr-ft²-°F | |
|
Eagle Brass 770 Nickel Silver 18%, Spring
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
|
|||