Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.900 - 1.00 W/m-K | 6.25 - 6.94 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |