Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.600 - 0.800 W/m-K | 4.16 - 5.55 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Thermal Conductivity | 0.600 - 0.800 W/m-K | 4.16 - 5.55 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Thermal Conductivity | 0.590 - 0.800 W/m-K | 4.09 - 5.55 BTU-in/hr-ft²-°F | Average value: 0.643 W/m-K Grade Count:6 |
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min.. |
|||
Thermal Conductivity | 0.277 - 0.800 W/m-K | 1.92 - 5.55 BTU-in/hr-ft²-°F | Average value: 0.540 W/m-K Grade Count:16 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |