Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.00 - 3.50 W/m-K | 20.8 - 24.3 BTU-in/hr-ft²-°F | Through Plane; ASTM E1461 |
PolyOne Trilliant™ HC HC6200-5001 XR Grey Polyamide 12 (Nylon 12) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Thermal Conductivity | 0.380 - 3.50 W/m-K | 2.64 - 24.3 BTU-in/hr-ft²-°F | Average value: 0.886 W/m-K Grade Count:15 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |