Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.280 - 0.310 W/m-K | 1.94 - 2.15 BTU-in/hr-ft²-°F | Average value: 0.294 W/m-K Grade Count:5 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Thermal Conductivity | 0.290 - 0.310 W/m-K @Temperature 100 - 250 °C |
2.01 - 2.15 BTU-in/hr-ft²-°F @Temperature 212 - 482 °F |
Average value: 0.300 W/m-K Grade Count:1 |
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum .. |
|||
Thermal Conductivity | 0.0400 - 0.310 W/m-K | 0.278 - 2.15 BTU-in/hr-ft²-°F | Average value: 0.203 W/m-K Grade Count:8 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |