Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 14.9 - 16.5 W/m-K | 103 - 115 BTU-in/hr-ft²-°F | after modified H900 heat treatment, XY direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Thermal Conductivity | 15.0 - 16.6 W/m-K | 104 - 115 BTU-in/hr-ft²-°F | Z (vertical) direction, after mod H900 heat treat |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Thermal Conductivity | 15.5 - 16.5 W/m-K | 108 - 115 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories Shelf Boards and Pillars SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |