Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 142 W/m-K | 985 BTU-in/hr-ft²-°F | comparable with pure Mo |
Plansee MoILQ Molybdenum Incandescent Light Quality Characteristics:Recrystallization temperature higher than pure MoFiner grain structure than pure MoApplications: This grade was developed for use in the lighting industry. It is more easily formed.. |
|||
Thermal Conductivity | 142 W/m-K | 985 BTU-in/hr-ft²-°F | comparable with pure Mo |
Plansee ML Molybdenum-Lanthanum Oxide Characteristics:"Stacked fiber" microstructureExtremely creep resistantApplications:Furnace components - wires, including stranded; sintering and annealing boats; evaporator coilsLighting - retainin.. |
|||
Thermal Conductivity | 142 W/m-K | 985 BTU-in/hr-ft²-°F | comparable with pure Mo |
Plansee MY Molybdenum-Yttrium-Cerium Oxide Characteristics:Greater resistance to oxidation than pure MoAdheres well to quartz glassEasily weldableApplications:Conductive ESS ribbonsCoating technology - evaporation boatsInformation provided b.. |
|||
Thermal Conductivity | 142 W/m-K | 985 BTU-in/hr-ft²-°F | |
Alcoa MIC-6 Aluminum Mold Alloy MIC-6 is a blend of the most desirable features of many individual metals. The result is a cast aluminum plate that meets the challenge of product accuracy demanded by today’s industry.Because of i.. |
|||
Thermal Conductivity | 142 W/m-K | 985 BTU-in/hr-ft²-°F | |
CMW® ELKON 100M Pure Molybdenum Molybdenum (ELKON® 100M) is a refractory metal that resembles tungsten in many respects. Its hardness, melting, and boiling temperatures are only slightly lower than those of tungsten are. The elec.. |
|||
Thermal Conductivity | 142 W/m-K | 985 BTU-in/hr-ft²-°F | comparable with pure Mo |
Plansee MLR Molybdenum-Lanthanum Oxide; Recrystallized Characteristics:"Stacked fiber" microstructureExtremely creep resistantApplications:Furnace components - wires, including stranded; sintering and annealing boats; evaporator coilsLighting - retainin.. |
|||
Thermal Conductivity | 142 W/m-K | 985 BTU-in/hr-ft²-°F | comparable with pure Mo |
Plansee MLS Molybdenum-Lanthanum Oxide; Stress Relieved Characteristics:"Stacked fiber" microstructureExtremely creep resistantApplications:Furnace components - wires, including stranded; sintering and annealing boats; evaporator coilsLighting - retainin.. |